默认 deteriorated masonry blocks - why

deteriorated masonry blocks - why?
saw a home this afternoon. contained masonry block foundation (actually appeared to be closer to the older cinderblock). home was constructed circa 1965 by what i have found out was a contractor of limited credentials. in the visible areas of the basement, every block, in the top row, was deteriorated, with numerous cracks and crumbling and powdering of the subcomponents. this damage was only limited to the top row. on the outside, the grade line was about 1/2 up this top row (another problem, but i digress). anyway, my thought is that the damage was due to moisture and thermal stresses - does anyone have an opinion on this? in addition, does anyone know a low-cost, but workable repair? the blocks have yet to show any extensive crushing, though there are likely some localized areas, since the sills and floor framing are bearing down.
thanks!
"spalling", this is caused by water freezing in the pores of the block, expanding and more or less reducing to block to powder or granular material.
is the block grouted solid? if so, it should not cause much of a structural problem unless the wall was of minimum strength to begin with. if all else is ok, suggest getting a qualified mason to offer an oppinion.
removing the source of moisture should be a priority, as this can lead to future problems.
if the top course of block is not grouted solid, then it should be. but, finding an easy way to do so is the kicker. many times the cores of the block are accessible from the inside, assuming this is a basement wall where you could get access. then it is a "simple" matter of stuffing some filler material into the core to below the first course and then filling the core up with grout. if the cores are not accessible, the job is less "simple".
thanks for the input. it was what i was thinking - sometimes one needs affirmation. enjoy the long weekend.
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
arching of masonry walls huangyhg 产品功能分析 0 2009-09-07 12:41 PM
allowable defelction for spandrel beam bracing masonry huangyhg 产品功能分析 0 2009-09-07 10:55 AM
【转帖】nested blocks yang686526 DirectDWG 0 2009-05-06 06:26 PM
【转帖】limitation on adding blocks to block table yang686526 DirectDWG 0 2009-05-06 04:47 PM
【转帖】import blocks yang686526 DirectDWG 0 2009-05-06 03:42 PM


所有的时间均为北京时间。 现在的时间是 05:56 AM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多