默认 weld strength

weld strength
what is the stronger of the two welds if they are used for welding the same thickness sheet of cusi plate? carbon arc or tig?
thanks for the info
before this question can be answered the following items need to be examined.
- joint design
- filler metals
- preheat and post weld heat treatment
- control of interpass temperature
- base metal cleaning techniques
- shape of weld - convex or concave
- heat input
- shielding and purge gases
- skill level of the welder
well you need to clarify you question a bit more than that.
what do you mean by carbon arc welding? i've seen sheet metal guys use carbon rods on straight polarity with "coat hanger"(sic), but what else do you mean?
at any rate, probably the best welds in most critical applications (pressure piping, nuclear facilities, refineries, etc.) are tig. it is slower and often difficult to implement in the field but consistently gives a near perfect weld in the hands of a professional.
this is not to say that stick or mig cannot yield "perfect" welds, they can and i have done my share but---that is not what you asked.
rod
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
 


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
weld end returns huangyhg 产品功能分析 0 2009-09-16 07:41 PM
max weld size question huangyhg 产品功能分析 0 2009-09-10 01:15 PM
concrete compressive strength huangyhg 产品功能分析 0 2009-09-08 11:53 AM
analysis of an over-weld huangyhg 产品功能分析 0 2009-09-07 11:35 AM
10 ft continuous weld beam to cover plate huangyhg 产品功能分析 0 2009-09-06 10:26 PM


所有的时间均为北京时间。 现在的时间是 01:19 AM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多