默认 why does standard welded wire mesh does not meet aci criteri

why does standard welded wire mesh does not meet aci criteri
hello fellow structural engineers,
this may be a dumb point, but 6x6 - w1.4xw1.4 wwm comes up woely short of the aci requirement of 0.0018.... in a 4" slab, wwm = 0.28 sq in/ft, but aci requires 0.0018*4*12 = 0.0864 sq in/ft.
what's that all about?
why does standard welded wire mesh that we always put in slabs not meet aci shrinkage & temperature criteria (7.12) for slabs with welded wire mesh? do the joints make up for it instead?
i guess 7.12 is for structural slabs only, and slab-on-grade is not meant to be included.
mike
read r7.12.1.
willisv,
so where are the minimum requirements for slab-on-grade?
seems like it's just owner/geotech preference?
mike
there is a subgrade drag formula (i can't re
yes, i heard the rule of thumb was 3 times the slab thicknes... i wasn't sure if there was still a minimum steel requirement... i'd never heard of one... just the better-than-nothing w1.4xw1.4 - 6x6 wwm.
to answer your questions, there are no minimum steel ratios for slab on grade. you design it as if it were unreinforced. the wire reinforcement is nominal and does not affect the strength. it is only there to keep cracking to a minimum width or try to at least. it also helps aggregate interlock at the joints. there is a somewhat new philosophy since there have been many lawsuits regarding slab for industrial and warehouse floors. the wire reinforcement you are using is fine for a 4" slab. it will never get to the location in the slab it is supposed to anyway.
the new aci 360-06 changes things again. they have even changed the name. it is now "welded wire reinforcement" (wwr)instead of welded wire fabric (wwf). it's more pc and marketable i guess. it's a chart for unreinforced but since the slab is only nominally reinforced, it is recommended to use these control joint spacings.
4" slab - about 8'
5" slab - about 12'
6" slab - about 14'
7" slab - about 16'
8" slab - about 17'
there are design methods in aci, pca, and wri. the wri are free to download. aci 360-06 contains them all. pca slabs on ground is a good book although dated a bit.
wri is the place to go. you'll "discover" that since wwr is usually of higher yield strength than regular grade 60 rebar and as such there's interesting conversions one can make and meet what the aci needs.
8' cj spacing in a 4" slab?!?!?
does anybody actually do this?
i really think the contractor would try to have architect all over me if i tried to make them install cj at 8'!
fwiw, my old firm probably puts in multiple million sq. ft. of 4" sog per year with a 20-30' (depending on the engineer) cj spacing and i've never heard of a problem.
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
welded wire fabric or mesh huangyhg 产品功能分析 0 2009-09-16 07:49 PM
【转帖】asme - where to star yang686526 American standards 0 2009-04-29 07:28 PM
【转帖】哪位高手指点一下下边lisp的怎么用 yang686526 数据库ObjectDBX 0 2009-04-28 12:13 PM
哪位高手指点一下下边lisp的怎么用 yang686526 ObjectARX(AutoLISP) 0 2009-04-26 06:19 PM
【转帖】asme美国机械工程师标准目录2 huangyhg American standards 5 2009-04-26 02:38 PM


所有的时间均为北京时间。 现在的时间是 03:58 AM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多