默认 weld question

weld question
i have a problem at a weld connection (gravity column to cap plate). the cap plate was 1" thick. the hss column had a 1/2" thickness. the weld specified was 5/16" (code minimum). the contractor used a 1/4" weld. is that fine or should i ask him to redo the weld.
find a job or post a job opening
the 13th edition steel specification revised the minimum, to match aws. under this code, the 1/4" weld does not violate this requirement, as it would be based on the thinner plate.
if 1/4" works for strength, i'd be inclined to leave it be.
i'm looking at the 13th edition and for a 1/2" piece, the min fillet weld is 3/16. i don't see a problem (unless you're not using low hydrogen rods - then you need to base it on the thicker part joined).
a 1/4" weld can be added to with ease, (another pass), not necessary if strength is sufficient using 1/4" weld.
the connection does work w/ a 1/4" weld.
this maybe a theoretical question, why is there a minimum size of weld for a particular thickness. does a smaller weld fail when connecting two thicker parts?

read the commentary in the manual.
it is a requirement based on the quenching effect of a thick piece of metal (even though the requirement is based on the thinner piece being joined).
a thick piece of metal rapidly conducts heat away from the weld, leading to rapid cooling which results in a loss of ductility.
since you are dealing with a minimum weld size, be sure to get the ones you have inspected by a certified welding inspector. a 1/4 inch fillet weld on thicker material is, as frv pointed out, subject to relatively fast cooling. depending on the welding process used, this can result in porosity, edge lap, lack of penetration, convexity, and lack of fusion.
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
weld end returns huangyhg 产品功能分析 0 2009-09-16 07:41 PM
max weld size question huangyhg 产品功能分析 0 2009-09-10 01:15 PM
flare weld vs. fillet weld question huangyhg 产品功能分析 0 2009-09-09 12:20 PM
10 ft continuous weld beam to cover plate huangyhg 产品功能分析 0 2009-09-06 10:26 PM
【转帖】ack weld a nu yang686526 American standards 0 2009-05-04 10:37 AM


所有的时间均为北京时间。 现在的时间是 11:06 PM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多