默认 wall reinforcement shadow lines

wall reinforcement shadow lines
good morning,
i have an odd question. we have a job that includes a wall with 2" of over on the outer most rebars. after form striping, you can see shadow lines of the resteel in the walls. anyone else run into this?
i have a couple ideas, but they seem far fetched.
a.
find a job or post a job opening
i saw this same thing on an elevated slab we did. the contractor said the rebar was hot when the concrete was poured, and the concrete around the bars dried and shrunk faster than the surrounding slab. it was over 100 degrees the day of the pour, and i imagine the bars baking in direct sun were even hotter. with a wall though, i would think the forms would keep things cool, and this hypothesis may not apply.
it could also be from form oil that was sprayed after the wall bars were placed, in which case the bars blocked the spray from the panels.
this is sometimes called "ghosting". wetting the surface will generally make it more noticeable.
typical on the back side of heavily reinforced tilt up walls, i was told it is an accumulation of fine aggregates on the underside of the steel when poured. cip wall, maybe a little less cover than spec'd.
i am inclined to think pmr06's suggestion about the form oil may be the answer, especially if the pattern you are seeing is both horizontal and vertical bars. would indicate that they forgot to oil the forms before placing the reinforcing mat. contractor should be able to tell you or find a worker who remembers.
if there was cracking along the horizontal bars, that would be poor consolidation and/or plastic settlement cracking.
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
vertical crack on foundation retaining wall huangyhg 产品功能分析 0 2009-09-16 06:18 PM
retaining wall failure huangyhg 产品功能分析 0 2009-09-15 06:38 PM
in enercalc masonry wall design, what is parapet heigh huangyhg 产品功能分析 0 2009-09-09 07:17 PM
foundation wall 40 feet below grade huangyhg 产品功能分析 0 2009-09-09 01:38 PM
concrete basement wall design huangyhg 产品功能分析 0 2009-09-08 11:39 AM