默认 help-garage slab

help-garage slab
ive done this calculation many times before in my old job but im on my own now and dont have any reference calcs. im doing something really stupid wrong but i cant figure it out. i have a large garage in a house with a basement under it. the max. span between filler beams is 9'. im using 18ga, 2" lok floor composite deck with a 5.5 inch slab. im using 60psf live and 60psf dead. my unshored construction spans are ok. my uniform loads are ok. i applied a concentrated load of 2000lb to the center of the span and my moment is huge. it is 4 times the uniform load moment per foot width. no slab will work with this, so im forgetting something. also, as i read ibc it seems to say you can design either for 50psf uniform load or 2000lb concentrated load. i would think this means, whichever is greater but it does not read this way. help..i need to get this done asap.
find a job or post a job opening
i think i figured it out. i found an example in the deck design book. but if anyone has any comments, let me know...
how much tributary slab width are you assuming resists the 2000 pound point load?
broekie,
thats what i thought the problem was but i couldnt get the numbers squared away in my head. after going through the example, i think it will be fine. the example was almost the exact same conditions.
jjeng2
i read the ibc the same way. you may use either one. i assume you have more than one span so use continuity and reinforce the slab over the support. other wise you will get cracks in the slab. the other choice is to use the steel deck as a form and use reinforcing in top and bottom of the slab. see the crsi handbook for one way slabs.
regards,
fepc
the usd catalog has an concentrated load example problem on page 19.
thanks lppe, thats the one i found.
i, too, am designing a suspended garage slab for a residential home. did anyone come up with an answer for the 2000 lb vs. 50 psf code scenario? as i read 2000 ibc, section 1607.4 states that you should compare the 2000 lb point load with the 50 psf uniform load and use the one that produces the greater load effect. as stated in the above thread, the 2000 lb point load always produces a much higher maximum moment on a simply supported structure. when the 2000 lb point load is used, the slab design seems terribly impractical from the suspended garage floors i have seen in the field for this application.
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
hairline cracks in post tensioned slab huangyhg 产品功能分析 0 2009-09-09 03:43 PM
garage slab over slab huangyhg 产品功能分析 0 2009-09-09 02:26 PM
elevated concretesteel beam garage slab design1 huangyhg 产品功能分析 0 2009-09-08 09:59 PM
cracks in two-way flat slab huangyhg 产品功能分析 0 2009-09-08 02:29 PM
crack in old floor slab huangyhg 产品功能分析 0 2009-09-08 02:20 PM


所有的时间均为北京时间。 现在的时间是 07:48 AM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多