默认 grade 60 bars..markings

grade 60 bars..markings
how can you tell if rebars are grade 60 or not. some have markings of "6" on them, but others do not, yet their mill certificates indicate grade 60. (of course i could be shown certs for grade 60 bars used elsewhere..)
one contractor insists that grade 40 bars break when bending, is there anything to this?
a pretty good explanation of rebar identification marks is at:
pt999,
reinforcing steel is marked this way.
there is two ways that bars are marked, one way is: when looking at the marks the top letter is the symbol for the producing mill (letter or symbol) the next is the bar size, a number such as six, meaning #6 bar, the next letter is the type of steel, the bar strength is indicated by a grade line (raised) parralel to the bar, no line means grade 40, one line means grade 60, and two lines means grade 75.
sometimes bars are noted right on the bar what grade it is such as 60, or 75, grade 40 would have no mark.
type of steel (third designation, below bar size):
s = billet meeting supplemental requirements si (a 615)
n = new billet (a 615)
r = for rail meeting astm a 617. grade 60 bend test requirement (a 616) [per aci 318-99]
a = axle (a 617)
w = low alloy (a 706)
__________________
借用达朗贝尔的名言:前进吧,你会得到信心!
[url="http://www.dimcax.com"]几何尺寸与公差标准[/url]
huangyhg离线中   回复时引用此帖
GDT自动化论坛(仅游客可见)
回复


主题工具 搜索本主题
搜索本主题:

高级搜索
显示模式

发帖规则
不可以发表新主题
不可以回复主题
不可以上传附件
不可以编辑您的帖子

vB 代码开启
[IMG]代码开启
HTML代码关闭

相似的主题
主题 主题发起者 论坛 回复 最后发表
concrete stair - nosing bars huangyhg 产品功能分析 0 2009-09-08 12:50 PM
bundled bars aci-02 7.6.6.2 requirement to enclose within s huangyhg 产品功能分析 0 2009-09-07 05:52 PM
8 inch and thicker slab on grade - one or two mats of steel huangyhg 产品功能分析 0 2009-09-07 08:58 AM
3d correct modeling huangyhg 产品功能分析 0 2009-09-07 08:41 AM
1927 concrete building huangyhg 产品功能分析 0 2009-09-06 10:39 PM


所有的时间均为北京时间。 现在的时间是 06:42 AM.


于2004年创办,几何尺寸与公差论坛"致力于产品几何量公差标准GD&T | GPS研究/CAD设计/CAM加工/CMM测量"。免责声明:论坛严禁发布色情反动言论及有关违反国家法律法规内容!情节严重者提供其IP,并配合相关部门进行严厉查处,若內容有涉及侵权,请立即联系我们QQ:44671734。注:此论坛须管理员验证方可发帖。
沪ICP备06057009号-2
更多