csa a23.1
i just need to know the %age of air content for both moderate and severe exposure for max. agg. sie 3/4" for freezing and thwing exposure
check out our whitepaper library.
5% to 8% seems optimum for high quality limestone aggregate.
from table 4 of a23.1
for category 1:
10mm agg: 6-9%
14-20mm agg: 5-8%
28-40mm agg: 4-7%
for category 2:
10mm agg: 5-8%
14-20mm agg: 4-7%
28-40mm agg: 3-6%