【转帖】cosmetic notes for hard black anodize
cosmetic notes for hard black anodize
i am looking for notes that call out cosmetic requirements related to hard black anodize. i need to put together a specification sheet so that production can determine if the parts they receive can be used or rejected because of plating flaws. get a copy of the spec mil-a-8625. it's all spelled out in it. like chris stated download a copy of mil-a-8625 it states qa processes and procedures. for example, section 4.4.2 calls out mil-std-105 for level ii inspection best regards, heckler sr. mechanical engineer sw2005 sp 5.0 & pro/e 2001 dell precision 370 p4 3.6 ghz, 1gb ram xp pro sp2.0 nvidia quadro fx 1400 o _`\(,_ (_)/ (_) never argue with an idiot. they'll bring you down to their level and beat you with experience every time. |